Home | About Us | Product | Know How | Contact Us |
|
|
|
|
ASTM A192/ASME SA192 Standard Specification for Seamless Carbon Steel Boiler Tubes for High-Pressure Service |
|
|
Standard: ASTM A192, ASME SA192
Equivalent Standards: EN 10216-1, EN 10216-2, DIN 17175, BS 3059 Part II, NF A 49-213, NBR 5594, GB 3087, GB 5310, JIS G3461 |
Material: SA192
Equivalent Materials: 1010, St35.8, 360, P195TR1 (1.0107), P195TR2 (1.0108), P195GH, 10#, 12G, STB340, 0.1-0.15C |
Chemistry Composition |
C, % |
Mn, % |
Si, % |
P, % |
S, % |
0.06-0.18 |
0.27-0.63 |
0.25 max |
0.035 max |
0.035 max |
|
Mechanical Properties |
Tensile Strength , MPa |
Yield Strength , MPa |
Elongation, % |
Hardness, HB, WT≥5.1mm |
Hardness, HRB, WT<5.1mm |
325 min |
180 min |
35 min |
137 max |
77 max |
|
Outside Diameter & Tolerance |
Hot rolled |
Outside Diameter, mm |
Tolerance, mm |
OD≤101.6 |
+0.4/-0.8 |
101.6<OD≤177.8 |
+0.4/-1.2 |
Cold Drawn |
Outside Diameter, mm |
Tolerance, mm |
OD<25.4 |
±0.10 |
25.4≤OD≤38.1 |
±0.15 |
38.1<OD<50.8 |
±0.20 |
50.8≤OD<63.5 |
±0.25 |
63.5≤OD<76.2 |
±0.30 |
76.2≤OD≤101.6 |
±0.38 |
101.6<OD≤177.8 |
+0.38/-0.64 |
|
Wall thickness & Tolerance |
Hot rolled
|
Outside Diameter, mm |
Tolerance, % |
OD≤101.6, WT≤2.4 |
+40/-0 |
OD≤101.6, 2.4<WT≤3.8 |
+35/-0 |
OD≤101.6, 3.8<WT≤4.6 |
+33/-0 |
OD≤101.6, WT>4.6 |
+28/-0 |
OD>101.6, 2.4<WT≤3.8 |
+35/-0 |
OD>101.6, 3.8<WT≤4.6 |
+33/-0 |
OD>101.6, WT>4.6 |
+28/-0 |
Cold Drawn
|
Outside Diameter, mm |
Tolerance, % |
OD≤38.1 |
+20/-0 |
OD>38.1 |
+22/-0 |
|
ASTM A192/A192M specifications covers minimum-wall-thickness, seamless carbon steel boiler and superheater tubes for high pressure service. The tubing sizes and thicknesses usually furnished to this specification are 1⁄2 in. to 7 in. [12.7 to 177.8 mm] outside diameter and 0.085 to 1.000 in. [2.2 to 25.4 mm], inclusive, in minimum wall thickness. Tubing having other dimensions may be furnished, provided such tubes comply with all other requirements of ASTM A192/A192M. |
Manufacture: tubes shall be made by the seamless process and shall be either hot-finished or cold-finished, as specified.
Heat Treatment: hot-finished tubes need not be heat treated. Cold finished tubes shall be heat treated after the final cold-finishing at a temperature of 1200°F [650°C] or higher.
Inspection & Test: chemistry composition analysis, tensile test, flattening test, flaring test, hardness test, NDT, surface inspection and dimension check. |
Length: 5800mm; 6000mm; 6096mm; 7315mm; 11800mm; and so on.
Max length: 30000mm, U bending can be offered, also see the fin tubes. |
Keyword: boiler steel pipes, ASTM A192, ASME SA192 |
|
|
|
|
|
|
|
Home | About Us | Product | Know How | Contact Us |
|